IMPRESSION CREEP TESTING MACHINE
Indian Institute of Technology (IIT) · Varanasi, Uttar Pradesh · Laboratory & Scientific Equipment · open
Key facts
- EMD: ₹50K
- Published: 02 Nov 2026
- Closing date: 24 Nov 2026
- Status: open
- Status as of: 04 Nov 2026 02:07 UTC
- Ministry: Ministry of Education
- Department: Department of Higher Education
- Office: Office of the Registrar, IIT (BHU), Varanasi
Description
Procurement of one impression creep testing machine for the School of Materials Science and Technology, IIT (BHU), Varanasi. Delivery is required within 60 days. The bid requires an EMD of Rs. 50,000 and performance security of 3% for 14 months.
Eligibility & requirements
- Experience required: 3 years
- Past performance: 80%
- Startup relaxation: Yes
- MSE relaxation: Yes
- Certifications: Valid Udyam Certificate, DPIIT Startup registration certificate (if claiming startup relaxation), OEM local content certificate
- Documents required: Experience Criteria, Past Performance, Bidder Turnover, Certificate (Requested in ATC), OEM Authorization Certificate, OEM Annual Turnover, Additional Doc 1 (Requested in ATC), Additional Doc 2 (Requested in ATC), Additional Doc 3 (Requested in ATC), Additional Doc 4 (Requested in ATC), Compliance of BoQ specification, Supporting document, Contracts and delivery acceptance certificates (e.g. CRAC) supporting experience, Certified audited balance sheets or Chartered Accountant/Cost Accountant turnover certificate, OEM certificate stating local content percentage and locations of local value addition
New to these terms? Read how tender eligibility criteria work.
Commercial terms
- Bid type: Two Packet Bid
- Evaluation: Total value wise evaluation
- Make in India (MII): Yes
- MSE preference: Yes
Line items (1)
- IMPRESSION CREEP TESTING MACHINE — Qty: 1 pieces
1 tender document(s) available — sign up to download.
Related tenders
- Supply of MERIL AUTO QUANT Biochemistry Reagents and Consumables — Laboratory & Scientific Equipment · Gujarat · ₹14.2L
- High Performance Automated Flash Chromatography — Laboratory & Scientific Equipment · Uttar Pradesh
- Supply of Items for Immunohistochemistry — Laboratory & Scientific Equipment · Assam · ₹3.0L
- E TENDER INVITED FOR SUPPLY OF AMCU ULTRASONIC MILK ANALYSER TOUCH SCREEN WITH OTP ENABLED AT PALI DAIRY SANGH — Laboratory & Scientific Equipment · Rajasthan · ₹1.2Cr
- Procurement of Consumables filter for Rion Lab water purification system Make Rion India for the Dept of Pharmacology on PAC Basis — Laboratory & Scientific Equipment · Odisha
- Procurement of Fluorescence Spectrometer — Laboratory & Scientific Equipment · Odisha · ₹1.6Cr
- Procurement of Pathology Laboratory Consumables and Reagents — Laboratory & Scientific Equipment · Dadra and Nagar Haveli and Daman and Diu
- Design Installation and Maintenance of Educational Lab/Centre - Science Lab; Site Preparation, Supply and Installation of Hardware, Furniture — Laboratory & Scientific Equipment · Jharkhand · ₹14.6L